Customized Test Conditions
The multi-functional design of the DEA 288 Ionic allows for the application of a great variety of different test conditions such as heat, cold or UV light. This enables the user to easily and conveniently determine the best parameters for processing the material.
A complete dielectric analyzer consists of the DEA electronics and a sensor. Disposable sensors are connected via an adaptor box. Four models of DEA 288 Ionic are available: the regular laboratory version and the slim version with small footprint and two industrial versions.
Both instruments are equipped with the same state-of-the-art electronics and have the ability to control additional accessories such as the lab furnace or lab press. The technical differences between the devices are in the design of the housing, the footprint and the maximum number of channels.
![](https://at-messe.netzsch.com/_Resources/Persistent/b/5/9/1/b5910186820d998a503cdea4eae525526ab4a3a4/DEA_288_Ionic_potable_version-2000x1333-600x400.webp)
DEA 288 Ionic
Portable Version
The portable version with up to 7 channels, this DEA is the flexible version for your day-to-day work. It can be easily transported between different measurement locations.
DEA 288 Ionic
Rack Version
The 19'' rack version is designed for an electrical cabinet. It supports 8 simultaneous measuring channels which can be extended to up to 16 modules.
![](https://at-messe.netzsch.com/_Resources/Persistent/0/9/4/c/094c36dcb2d126ba1028dd717c14ba2647441ed2/DEA_288_Ionic_Rack_Version_03-2000x1333-600x400.webp)
Technical Data
Frequency range
Data acquisition multiple DEA modules
Minimum data acquisition time
![](https://at-messe.netzsch.com/_Resources/Persistent/1/1/4/8/114827be33a71d95164cd2fb9a8b9c62b0bef9d9/DEA_288_Ionic_Portable_with_adapter_box_TMCc_sensor-2000x1333-600x400.webp)
Sensor connection
Shielded 4-wire technique (compensation of resistivity and capacity of the wire as a prerequisite for precise measurements)
DEA modules
Portable Version: All-purpose version, up to 7 channels
Industrial Rack Version: up to 8 channels (extension possible for up to 16 channels)
I/O Ports
Input and output of measuring signals or signals from peripheral devices such as pressure or temperature sensors. DEA allows for triggering by manufacturing machines.
![](https://at-messe.netzsch.com/_Resources/Persistent/3/8/a/0/38a025b60dcf1154708b53ab1201f3279eb63a16/netzs.ch_contactform.png)
GET IN CONTACT
Scan the QR-Code with your smartphone
You still have questions and would like to be contacted by our sales department? Would you like to receive a quote for the product? Do you need a poster or brochure for one of our products? Just Scan the QR-Code!