The DMA GABO EPLEXOR HT line is the only instrument series on the market which is able to carry out DMA measurements with a maximum dynamic force of 500 N to 1500°C.
Two high-temperature furnaces are available: RT to 1000°C and RT to 1500°C. With a standard furnace (-160°C to 500°C) simultaneously mounted, it is possible to perform consecutive test runs in both the low- and high-temperature range. EPLEXOR HT instruments can thus cover the entire temperature span from -160°C to 1500°C.
The electronics within the system automatically identify which furnace is currently in use.
The following DMA GABO EPLEXOR HT are available:
Instrument Type | Max. Static Force | Max. Dynamic Force *) |
---|---|---|
DMA GABO EPLEXOR 25N HT | 1500 N | ± 25 N |
DMA GABO EPLEXOR 100N HT | 1500 N | ± 100 N |
DMA GABO EPLEXOR 150N HT | 1500 N | ± 150 N |
DMA GABO EPLEXOR 500N HT | 1500 N | ± 500 N |
Technical Data
Temperature range
Static force range
Frequency range
200 Hz
![](https://at-messe.netzsch.com/_Resources/Persistent/2/9/a/9/29a9d0934ded24edb4de0545c78279d502dd897f/DMA_GABO_EPLEXOR_HT_02-600x600.webp)
- Dynamic force range:
from ± 25 N up to ± 500 N (depending on instrument type, see table) - Force sensor:
interchangeable; nominal forces available from 10 N to 500 N (depending on the instrument type and configuration) - Static displacement:
max. 60 mm - Dynamic amplitude:
from ± 1.5 mm up to ± 6 mm (depending on the instrument type and system configuration) - Measurement modes for applications above 500°C:
asymmetric and 3/4-point bending, compression - Work space of the high-temperature furnaces:
cylindrical chamber, diameter: 70 mm, height: 120 mm
![](https://at-messe.netzsch.com/_Resources/Persistent/3/8/a/0/38a025b60dcf1154708b53ab1201f3279eb63a16/netzs.ch_contactform.png)
GET IN CONTACT
Scan the QR-Code with your smartphone
You still have questions and would like to be contacted by our sales department? Would you like to receive a quote for the product? Do you need a poster or brochure for one of our products? Just Scan the QR-Code!