Accurate measurements of heat build-up or blowout processes and the determination of the thermal set can be realised by our HBU 523 Gabometer system – a development based on the established Goodrich Flexometer.
Both force- and elongation-controlled tests can be carried out with this state-of-the-art type of flexometer. The HBU 523 Gabometer is suitable for improving the thermal dissipation and the durability of semi-finished tire components, dampers or absorbers.
Additionally, the new generation allows for measurement of the material stiffness (E modulus, tanδ option) and damping.
Your Advantages
- Heat build-up and blowout tests according to Goodrich (DIN 53533, ASTM D 623, ISO 4666/3, ISO 4666/4, BS 903 part A50 and JIS K 6265)
- Goodrich flexometer tests
- Static: strain or stress controlled load mode available
- Dynamic: strain or stress controlled load mode available
- Wide frequency range (option)
- Wide temperature range (option)
![](https://at-messe.netzsch.com/_Resources/Persistent/b/f/1/0/bf10b7fafb6429868d0579b13c2ed8e25dbf925e/DMS%20523%20Explexor%203-156-7680x5120-600x400.webp)
- Automatic Sample Changer (ASC) for fully automatic testing (24h) (option)
- Simultaneous measurement of the visco-elastic properties (option)
- Visco-elastic properties in DMTS/DMA mode (option)
- Hysteresis analysis (option)
- Pulse load mode available (option)
Technical Data
Dynamic Strain Range
Static Deformation
Frequency Range
0.0001 Hz to 100 Hz (optional)
![](https://at-messe.netzsch.com/_Resources/Persistent/a/a/a/f/aaaf769aa09ff170112444b2c41f2e1df2d3247b/DMA_523_Eplexor_05_en-600x853.webp)
- Temperature Range:
-160°C up to 300°C - Test Specimen Size:
Diameter: up to 30 mm (optional < 40 mm), depending on model
Length: 25 mm
![](https://at-messe.netzsch.com/_Resources/Persistent/3/8/a/0/38a025b60dcf1154708b53ab1201f3279eb63a16/netzs.ch_contactform.png)
GET IN CONTACT
Scan the QR-Code with your smartphone
You still have questions and would like to be contacted by our sales department? Would you like to receive a quote for the product? Do you need a poster or brochure for one of our products? Just Scan the QR-Code!