State-of-the-art technology for thermophysical properties
The NETZSCH LFA 457 MicroFlash complies with the latest technology for modern laser flash systems. The table-top instrument allows measurements from -125°C to 1100°C using two different user-exchangeable furnaces.
The innovative infrared sensor technology employed in the system enables measurement of the temperature increase on the back surface of the sample, even at temperatures of -125°C.
The instrument can be used for small and large sample sizes of up to 25.4 mm diameter and, with the integrated sample changer, measurements can be run on several samples at the same time.
The vacuum-tight design enables tests under defined atmospheres.
The vertical arrangement of the sample holder, furnace and detector simplifies sample placement and, at the same time, guarantees an optimum signal-to-noise ratio of the detector signal.
The LFA 457 MicroFlash is the most up-to-date and versatile LFA system for research and development and for all applications involving characterization of standard and high-performance materials in automobile manufacturing, aeronautics, astronautics and energy technology.
Technical Data
Temperature range
(2 exchangeable furnace types)
Heating- and cooling rates
Laser pulse energy
![](https://at-messe.netzsch.com/_Resources/Persistent/0/5/5/6/05568f31fab3c1f10e86dad7d13e8e6963fff7a0/LFA_457_1-473x473-473x473.webp)
Measuring range:
0.01 mm2/s to 1000 mm2/s (thermal diffusivity)
Measuring range:
0.1 W/mK to 2000 W/mK (thermal conductivity)
Sample dimensions:
10 mm to 25.4 mm diameter (also 8x8 mm and 10x10 mm, square)
0.1 mm to 6 mm thickness
Sample holder:
SiC, graphite
Liquid metal holder: sapphire
Sample holder for liquids: platinum
Atmosphere:
inert, oxidizing, reducing, static, dynamic
Vacuum-tight assembly
up to 10-2 mbar (1 Pa)
![](https://at-messe.netzsch.com/_Resources/Persistent/0/1/5/d/015d694eb69844431277e6c1218275df7175f251/LFA_457_MicroFlash_1-600x600.webp)
![](https://at-messe.netzsch.com/_Resources/Persistent/3/8/a/0/38a025b60dcf1154708b53ab1201f3279eb63a16/netzs.ch_contactform.png)
GET IN CONTACT
Scan the QR-Code with your smartphone
You still have questions and would like to be contacted by our sales department? Would you like to receive a quote for the product? Do you need a poster or brochure for one of our products? Just Scan the QR-Code!