Technical Data DSC 300 Caliris
Maximum Temperature Range
Maximum Heating Rate
Automatic Sample Changer

Enthalpy precision (H-Module):
± 0.05% for indium
Temperature precision (H- and P-Module):
± 0.01 K (standard deviation from mean value, indium)
Temperature accuracy (H-Module):
± 0.05 K (Indium)
Peak-to-peak noise ratio:
± 2 µW
Repeatability:
± 0.3% (peak area; In, C10H16, Zn)
Gas atmospheres:
Inert, oxidizing, static and dynamic
The future is now!
Bring our devices into your laboratory with the click of a button.
Simply scan the QR code and get a 3D model of the instrument directly on your mobile phone or tablet. With the help of the latest AR Technology (Artificial Reality), the 3D model can easily be placed in your laboratory in its original life size. This function is browser-based and requires no app. Rollwiderstand
Find out and be amazed!
Download brochure

Get our FREE newsletter

Cooling options:
- Compressed air cooling (RT to 650°C/750°C)
- Vortex tube (compressed air): < 0°C to 650°C/750°C
- Compressed air with switch valve RT to 650°C/750°C
- IC40 (-40°C to 600°C)
- IC70 (-70°C to 600°C)
- IC90 (-90°C to 600°C)
- LN2 (-180°C to 650°C/750°C)
Heating/cooling rate:
- H-Module: 0.001 K/min to 200 K/min
- P-Module: 0.001 K/min to 500 K/min
(Maximum rates depend upon end temperature) - S-Module: 0.001 K/min to 100 K/min